cmos61PVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mp10x0.8 |
Avg. Threshhold Voltage=-0.653 |
Avg. Sigma=0.014 |
|---|
| Mp5x0.8 |
Avg. Threshhold Voltage=-0.697 |
Avg. Sigma=0.015 |
|---|
| Mp15x0.8 |
Avg. Threshhold Voltage=-0.642 |
Avg. Sigma=0.014 |
|---|
| Mp10x0.9 |
Avg. Threshhold Voltage=-0.676 |
Avg. Sigma=0.012 |
|---|
| Mp5x0.9 |
Avg. Threshhold Voltage=-0.713 |
Avg. Sigma=0.020 |
|---|
| Mp15x0.9 |
Avg. Threshhold Voltage=-0.673 |
Avg. Sigma=0.015 |
|---|
| Mp5x1.0 |
Avg. Threshhold Voltage=-0.720 |
Avg. Sigma=0.013 |
|---|
| Mp10x1.0 |
Avg. Threshhold Voltage=-0.696 |
Avg. Sigma=0.010 |
|---|
| Mp15x1.0 |
Avg. Threshhold Voltage=-0.688 |
Avg. Sigma=0.011 |
|---|
| Mp5x1.1 |
Avg. Threshhold Voltage=-0.723 |
Avg. Sigma=0.011 |
|---|
| Mp10x1.1 |
Avg. Threshhold Voltage=-0.702 |
Avg. Sigma=0.011 |
|---|
| Mp15x1.1 |
Avg. Threshhold Voltage=-0.697 |
Avg. Sigma=0.012 |
|---|
| Mp5x1.2 |
Avg. Threshhold Voltage=-0.725 |
Avg. Sigma=0.012 |
|---|
| Mp10x1.2 |
Avg. Threshhold Voltage=-0.707 |
Avg. Sigma=0.011 |
|---|
| Mp15x1.2 |
Avg. Threshhold Voltage=-0.701 |
Avg. Sigma=0.011 |
|---|
| Mp10x2 |
Avg. Threshhold Voltage=-0.718 |
Avg. Sigma=0.010 |
|---|
| Mp5x2 |
Avg. Threshhold Voltage=-0.732 |
Avg. Sigma=0.011 |
|---|
| Mp15x2 |
Avg. Threshhold Voltage=-0.715 |
Avg. Sigma=0.011 |
|---|
| Mp10x3 |
Avg. Threshhold Voltage=-0.719 |
Avg. Sigma=0.009 |
|---|
| Mp5x3 |
Avg. Threshhold Voltage=-0.733 |
Avg. Sigma=0.010 |
|---|
| Mp15x3 |
Avg. Threshhold Voltage=-0.716 |
Avg. Sigma=0.013 |
|---|
| Mp5x5 |
Avg. Threshhold Voltage=-0.729 |
Avg. Sigma=0.008 |
|---|
| Mp10x5 |
Avg. Threshhold Voltage=-0.717 |
Avg. Sigma=0.010 |
|---|
| Mp15x5 |
Avg. Threshhold Voltage=-0.714 |
Avg. Sigma=0.010 |
|---|