cmos61NVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mn10x0.8 |
Avg. Threshhold Voltage=0.696 |
Avg. Sigma=0.012 |
|---|
| Mn5x0.8 |
Avg. Threshhold Voltage=0.703 |
Avg. Sigma=0.019 |
|---|
| Mn15x0.8 |
Avg. Threshhold Voltage=0.690 |
Avg. Sigma=0.013 |
|---|
| Mn10x0.9 |
Avg. Threshhold Voltage=0.697 |
Avg. Sigma=0.010 |
|---|
| Mn5x0.9 |
Avg. Threshhold Voltage=0.712 |
Avg. Sigma=0.013 |
|---|
| Mn15x0.9 |
Avg. Threshhold Voltage=0.699 |
Avg. Sigma=0.010 |
|---|
| Mn5x1.0 |
Avg. Threshhold Voltage=0.713 |
Avg. Sigma=0.020 |
|---|
| Mn10x1.0 |
Avg. Threshhold Voltage=0.700 |
Avg. Sigma=0.016 |
|---|
| Mn15x1.0 |
Avg. Threshhold Voltage=0.700 |
Avg. Sigma=0.008 |
|---|
| Mn5x1.1 |
Avg. Threshhold Voltage=0.720 |
Avg. Sigma=0.008 |
|---|
| Mn10x1.1 |
Avg. Threshhold Voltage=0.708 |
Avg. Sigma=0.042 |
|---|
| Mn15x1.1 |
Avg. Threshhold Voltage=0.701 |
Avg. Sigma=0.009 |
|---|
| Mn5x1.2 |
Avg. Threshhold Voltage=0.735 |
Avg. Sigma=0.054 |
|---|
| Mn10x1.2 |
Avg. Threshhold Voltage=0.703 |
Avg. Sigma=0.010 |
|---|
| Mn15x1.2 |
Avg. Threshhold Voltage=0.704 |
Avg. Sigma=0.008 |
|---|
| Mn10x2 |
Avg. Threshhold Voltage=0.719 |
Avg. Sigma=0.036 |
|---|
| Mn5x2 |
Avg. Threshhold Voltage=0.728 |
Avg. Sigma=0.068 |
|---|
| Mn15x2 |
Avg. Threshhold Voltage=0.705 |
Avg. Sigma=0.010 |
|---|
| Mn10x3 |
Avg. Threshhold Voltage=0.710 |
Avg. Sigma=0.005 |
|---|
| Mn5x3 |
Avg. Threshhold Voltage=0.720 |
Avg. Sigma=0.007 |
|---|
| Mn15x3 |
Avg. Threshhold Voltage=0.702 |
Avg. Sigma=0.011 |
|---|
| Mn5x5 |
Avg. Threshhold Voltage=0.727 |
Avg. Sigma=0.047 |
|---|
| Mn10x5 |
Avg. Threshhold Voltage=0.707 |
Avg. Sigma=0.008 |
|---|
| Mn15x5 |
Avg. Threshhold Voltage=0.705 |
Avg. Sigma=0.005 |
|---|