cmos60Resist
| STRUCTURE NAME | AVG. SHEET RESISTANCE | AVG. SIGMA |
| conrp+ |
Avg. sheet Resistance=0.023 |
Avg. Sigma=0.010 |
|---|
| conrn+ |
Avg. sheet Resistance=0.019 |
Avg. Sigma=0.007 |
|---|
| conrpo |
Avg. sheet Resistance=0.0 |
Avg. Sigma=0.0 |
|---|
| conrm2 |
Avg. sheet Resistance=0.0 |
Avg. Sigma=0.0 |
|---|