cmos60PVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mp10x0.8 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp5x0.8 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp15x0.8 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp10x0.9 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp5x0.9 |
Avg. Threshhold Voltage=0.017 |
Avg. Sigma=0.1507 |
|---|
| Mp15x0.9 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp5x1.0 |
Avg. Threshhold Voltage=-0.137 |
Avg. Sigma=0.102 |
|---|
| Mp10x1.0 |
Avg. Threshhold Voltage=-0.013 |
Avg. Sigma=0.094 |
|---|
| Mp15x1.0 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp5x1.1 |
Avg. Threshhold Voltage=-0.125 |
Avg. Sigma=0.130 |
|---|
| Mp10x1.1 |
Avg. Threshhold Voltage=-0.115 |
Avg. Sigma=0.113 |
|---|
| Mp15x1.1 |
Avg. Threshhold Voltage=0.0 |
Avg. Sigma=0.0 |
|---|
| Mp5x1.2 |
Avg. Threshhold Voltage=-0.181 |
Avg. Sigma=0.130 |
|---|
| Mp10x1.2 |
Avg. Threshhold Voltage=-0.141 |
Avg. Sigma=0.127 |
|---|
| Mp15x1.2 |
Avg. Threshhold Voltage=-0.202 |
Avg. Sigma=0.086 |
|---|
| Mp10x2 |
Avg. Threshhold Voltage=-0.351 |
Avg. Sigma=0.070 |
|---|
| Mp5x2 |
Avg. Threshhold Voltage=-0.395 |
Avg. Sigma=0.056 |
|---|
| Mp15x2 |
Avg. Threshhold Voltage=-0.349 |
Avg. Sigma=0.077 |
|---|
| Mp10x3 |
Avg. Threshhold Voltage=-0.380 |
Avg. Sigma=0.072 |
|---|
| Mp5x3 |
Avg. Threshhold Voltage=-0.412 |
Avg. Sigma=0.071 |
|---|
| Mp15x3 |
Avg. Threshhold Voltage=-0.380 |
Avg. Sigma=0.077 |
|---|
| Mp5x5 |
Avg. Threshhold Voltage=-0.417 |
Avg. Sigma=0.068 |
|---|
| Mp10x5 |
Avg. Threshhold Voltage=-0.524 |
Avg. Sigma=0.030 |
|---|
| Mp15x5 |
Avg. Threshhold Voltage=-0.386 |
Avg. Sigma=0.077 |
|---|