| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mn10x0.8 |
Avg. Threshhold Voltage=0.600 |
Avg. Sigma=0.0 |
|---|
| Mn5x0.8 |
Avg. Threshhold Voltage=0.605 |
Avg. Sigma=0.027 |
|---|
| Mn15x0.8 |
Avg. Threshhold Voltage=0.596 |
Avg. Sigma=0.0 |
|---|
| Mn10x0.9 |
Avg. Threshhold Voltage=0.654 |
Avg. Sigma=0.038 |
|---|
| Mn5x0.9 |
Avg. Threshhold Voltage=0.648 |
Avg. Sigma=0.039 |
|---|
| Mn15x0.9 |
Avg. Threshhold Voltage=0.666 |
Avg. Sigma=0.033 |
|---|
| Mn5x1.0 |
Avg. Threshhold Voltage=0.723 |
Avg. Sigma=0.022 |
|---|
| Mn10x1.0 |
Avg. Threshhold Voltage=0.716 |
Avg. Sigma=0.026 |
|---|
| Mn15x1.0 |
Avg. Threshhold Voltage=0.718 |
Avg. Sigma=0.024 |
|---|
| Mn5x1.1 |
Avg. Threshhold Voltage=0.746 |
Avg. Sigma=0.017 |
|---|
| Mn10x1.1 |
Avg. Threshhold Voltage=0.744 |
Avg. Sigma=0.016 |
|---|
| Mn15x1.1 |
Avg. Threshhold Voltage=0.745 |
Avg. Sigma=0.016 |
|---|
| Mn5x1.2 |
Avg. Threshhold Voltage=0.756 |
Avg. Sigma=0.025 |
|---|
| Mn10x1.2 |
Avg. Threshhold Voltage=0.752 |
Avg. Sigma=0.012 |
|---|
| Mn15x1.2 |
Avg. Threshhold Voltage=0.753 |
Avg. Sigma=0.012 |
|---|
| Mn10x2 |
Avg. Threshhold Voltage=0.758 |
Avg. Sigma=0.006 |
|---|
| Mn5x2 |
Avg. Threshhold Voltage=0.763 |
Avg. Sigma=0.008 |
|---|
| Mn15x2 |
Avg. Threshhold Voltage=0.757 |
Avg. Sigma=0.005 |
|---|
| Mn10x3 |
Avg. Threshhold Voltage=0.747 |
Avg. Sigma=0.005 |
|---|
| Mn5x3 |
Avg. Threshhold Voltage=0.752 |
Avg. Sigma=0.006 |
|---|
| Mn15x3 |
Avg. Threshhold Voltage=0.746 |
Avg. Sigma=0.005 |
|---|
| Mn5x5 |
Avg. Threshhold Voltage=0.745 |
Avg. Sigma=0.005 |
|---|
| Mn10x5 |
Avg. Threshhold Voltage=0.738 |
Avg. Sigma=0.005 |
|---|
| Mn15x5 |
Avg. Threshhold Voltage=0.736 |
Avg. Sigma=0.005 |
|---|