| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mp10x0.8 |
Avg. Threshhold Voltage=-0.767 |
Avg. Sigma=0.018 |
|---|
| Mp5x0.8 |
Avg. Threshhold Voltage=-0.822 |
Avg. Sigma=0.037 |
|---|
| Mp15x0.8 |
Avg. Threshhold Voltage=-0.764 |
Avg. Sigma=0.015 |
|---|
| Mp10x0.9 |
Avg. Threshhold Voltage=-0.794 |
Avg. Sigma=0.017 |
|---|
| Mp5x0.9 |
Avg. Threshhold Voltage=-0.870 |
Avg. Sigma=0.027 |
|---|
| Mp15x0.9 |
Avg. Threshhold Voltage=-0.789 |
Avg. Sigma=0.014 |
|---|
| Mp5x1.0 |
Avg. Threshhold Voltage=-0.890 |
Avg. Sigma=0.032 |
|---|
| Mp10x1.0 |
Avg. Threshhold Voltage=-0.805 |
Avg. Sigma=0.017 |
|---|
| Mp15x1.0 |
Avg. Threshhold Voltage=-0.798 |
Avg. Sigma=0.013 |
|---|
| Mp5x1.1 |
Avg. Threshhold Voltage=-0.886 |
Avg. Sigma=0.023 |
|---|
| Mp10x1.1 |
Avg. Threshhold Voltage=-0.815 |
Avg. Sigma=0.016 |
|---|
| Mp15x1.1 |
Avg. Threshhold Voltage=-0.806 |
Avg. Sigma=0.014 |
|---|
| Mp5x1.2 |
Avg. Threshhold Voltage=-0.889 |
Avg. Sigma=0.022 |
|---|
| Mp10x1.2 |
Avg. Threshhold Voltage=-0.822 |
Avg. Sigma=0.018 |
|---|
| Mp15x1.2 |
Avg. Threshhold Voltage=-0.812 |
Avg. Sigma=0.015 |
|---|
| Mp10x2 |
Avg. Threshhold Voltage=-0.839 |
Avg. Sigma=0.018 |
|---|
| Mp5x2 |
Avg. Threshhold Voltage=-0.926 |
Avg. Sigma=0.017 |
|---|
| Mp15x2 |
Avg. Threshhold Voltage=-0.824 |
Avg. Sigma=0.014 |
|---|
| Mp10x3 |
Avg. Threshhold Voltage=-0.839 |
Avg. Sigma=0.012 |
|---|
| Mp5x3 |
Avg. Threshhold Voltage=-0.871 |
Avg. Sigma=0.015 |
|---|
| Mp15x3 |
Avg. Threshhold Voltage=-0.833 |
Avg. Sigma=0.014 |
|---|
| Mp5x5 |
Avg. Threshhold Voltage=-0.871 |
Avg. Sigma=0.014 |
|---|
| Mp10x5 |
Avg. Threshhold Voltage=-0.843 |
Avg. Sigma=0.015 |
|---|
| Mp15x5 |
Avg. Threshhold Voltage=-0.838 |
Avg. Sigma=0.013 |
|---|