cmos59bNVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mn10x0.8 |
Avg. Threshhold Voltage=0.778 |
Avg. Sigma=0.023 |
|---|
| Mn5x0.8 |
Avg. Threshhold Voltage=0.924 |
Avg. Sigma=0.060 |
|---|
| Mn15x0.8 |
Avg. Threshhold Voltage=0.773 |
Avg. Sigma=0.014 |
|---|
| Mn10x0.9 |
Avg. Threshhold Voltage=0.781 |
Avg. Sigma=0.024 |
|---|
| Mn5x0.9 |
Avg. Threshhold Voltage=0.946 |
Avg. Sigma=0.066 |
|---|
| Mn15x0.9 |
Avg. Threshhold Voltage=0.773 |
Avg. Sigma=0.015 |
|---|
| Mn5x1.0 |
Avg. Threshhold Voltage=0.983 |
Avg. Sigma=0.067 |
|---|
| Mn10x1.0 |
Avg. Threshhold Voltage=0.782 |
Avg. Sigma=0.021 |
|---|
| Mn15x1.0 |
Avg. Threshhold Voltage=0.774 |
Avg. Sigma=0.011 |
|---|
| Mn5x1.1 |
Avg. Threshhold Voltage=0.989 |
Avg. Sigma=0.069 |
|---|
| Mn10x1.1 |
Avg. Threshhold Voltage=0.784 |
Avg. Sigma=0.020 |
|---|
| Mn15x1.1 |
Avg. Threshhold Voltage=0.773 |
Avg. Sigma=0.014 |
|---|
| Mn5x1.2 |
Avg. Threshhold Voltage=1.012 |
Avg. Sigma=0.066 |
|---|
| Mn10x1.2 |
Avg. Threshhold Voltage=0.787 |
Avg. Sigma=0.021 |
|---|
| Mn15x1.2 |
Avg. Threshhold Voltage=0.774 |
Avg. Sigma=0.013 |
|---|
| Mn10x2 |
Avg. Threshhold Voltage=0.781 |
Avg. Sigma=0.019 |
|---|
| Mn5x2 |
Avg. Threshhold Voltage=1.047 |
Avg. Sigma=0.084 |
|---|
| Mn15x2 |
Avg. Threshhold Voltage=0.770 |
Avg. Sigma=0.014 |
|---|
| Mn10x3 |
Avg. Threshhold Voltage=0.782 |
Avg. Sigma=0.025 |
|---|
| Mn5x3 |
Avg. Threshhold Voltage=1.011 |
Avg. Sigma=0.117 |
|---|
| Mn15x3 |
Avg. Threshhold Voltage=0.768 |
Avg. Sigma=0.014 |
|---|
| Mn5x5 |
Avg. Threshhold Voltage=0.934 |
Avg. Sigma=0.138 |
|---|
| Mn10x5 |
Avg. Threshhold Voltage=0.784 |
Avg. Sigma=0.033 |
|---|
| Mn15x5 |
Avg. Threshhold Voltage=0.766 |
Avg. Sigma=0.019 |
|---|