cmos58PVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mp10x0.8 |
Avg. Threshhold Voltage=-0.685 |
Avg. Sigma=0.058 |
|---|
| Mp5x0.8 |
Avg. Threshhold Voltage=-0.631 |
Avg. Sigma=0.063 |
|---|
| Mp15x0.8 |
Avg. Threshhold Voltage=-0.743 |
Avg. Sigma=0.030 |
|---|
| Mp10x0.9 |
Avg. Threshhold Voltage=-0.776 |
Avg. Sigma=0.029 |
|---|
| Mp5x0.9 |
Avg. Threshhold Voltage=-0.723 |
Avg. Sigma=0.058 |
|---|
| Mp15x0.9 |
Avg. Threshhold Voltage=-0.791 |
Avg. Sigma=0.022 |
|---|
| Mp5x1.0 |
Avg. Threshhold Voltage=-0.801 |
Avg. Sigma=0.033 |
|---|
| Mp10x1.0 |
Avg. Threshhold Voltage=-0.819 |
Avg. Sigma=0.019 |
|---|
| Mp15x1.0 |
Avg. Threshhold Voltage=-0.824 |
Avg. Sigma=0.017 |
|---|
| Mp5x1.1 |
Avg. Threshhold Voltage=-0.825 |
Avg. Sigma=0.026 |
|---|
| Mp10x1.1 |
Avg. Threshhold Voltage=-0.838 |
Avg. Sigma=0.017 |
|---|
| Mp15x1.1 |
Avg. Threshhold Voltage=-0.842 |
Avg. Sigma=0.013 |
|---|
| Mp5x1.2 |
Avg. Threshhold Voltage=-0.846 |
Avg. Sigma=0.023 |
|---|
| Mp10x1.2 |
Avg. Threshhold Voltage=-0.850 |
Avg. Sigma=0.016 |
|---|
| Mp15x1.2 |
Avg. Threshhold Voltage=-0.852 |
Avg. Sigma=0.013 |
|---|
| Mp10x2 |
Avg. Threshhold Voltage=-0.884 |
Avg. Sigma=0.011 |
|---|
| Mp5x2 |
Avg. Threshhold Voltage=-0.899 |
Avg. Sigma=0.017 |
|---|
| Mp15x2 |
Avg. Threshhold Voltage=-0.882 |
Avg. Sigma=0.010 |
|---|
| Mp10x3 |
Avg. Threshhold Voltage=-0.891 |
Avg. Sigma=0.011 |
|---|
| Mp5x3 |
Avg. Threshhold Voltage=-0.904 |
Avg. Sigma=0.016 |
|---|
| Mp15x3 |
Avg. Threshhold Voltage=-0.886 |
Avg. Sigma=0.009 |
|---|
| Mp5x5 |
Avg. Threshhold Voltage=-0.923 |
Avg. Sigma=0.094 |
|---|
| Mp10x5 |
Avg. Threshhold Voltage=-0.890 |
Avg. Sigma=0.010 |
|---|
| Mp15x5 |
Avg. Threshhold Voltage=-0.886 |
Avg. Sigma=0.008 |
|---|