cmos58NVT
| STRUCTURE NAME | AVG. THRESHHOLD VOLTAGE | AVG. SIGMA |
| Mn10x0.8 |
Avg. Threshhold Voltage=0.756 |
Avg. Sigma=0.015 |
|---|
| Mn5x0.8 |
Avg. Threshhold Voltage=0.759 |
Avg. Sigma=0.042 |
|---|
| Mn15x0.8 |
Avg. Threshhold Voltage=0.754 |
Avg. Sigma=0.015 |
|---|
| Mn10x0.9 |
Avg. Threshhold Voltage=0.763 |
Avg. Sigma=0.014 |
|---|
| Mn5x0.9 |
Avg. Threshhold Voltage=0.768 |
Avg. Sigma=0.021 |
|---|
| Mn15x0.9 |
Avg. Threshhold Voltage=0.760 |
Avg. Sigma=0.016 |
|---|
| Mn5x1.0 |
Avg. Threshhold Voltage=0.776 |
Avg. Sigma=0.017 |
|---|
| Mn10x1.0 |
Avg. Threshhold Voltage=0.768 |
Avg. Sigma=0.013 |
|---|
| Mn15x1.0 |
Avg. Threshhold Voltage=0.763 |
Avg. Sigma=0.015 |
|---|
| Mn5x1.1 |
Avg. Threshhold Voltage=0.774 |
Avg. Sigma=0.017 |
|---|
| Mn10x1.1 |
Avg. Threshhold Voltage=0.764 |
Avg. Sigma=0.013 |
|---|
| Mn15x1.1 |
Avg. Threshhold Voltage=0.760 |
Avg. Sigma=0.012 |
|---|
| Mn5x1.2 |
Avg. Threshhold Voltage=0.775 |
Avg. Sigma=0.016 |
|---|
| Mn10x1.2 |
Avg. Threshhold Voltage=0.765 |
Avg. Sigma=0.012 |
|---|
| Mn15x1.2 |
Avg. Threshhold Voltage=0.757 |
Avg. Sigma=0.013 |
|---|
| Mn10x2 |
Avg. Threshhold Voltage=0.753 |
Avg. Sigma=0.010 |
|---|
| Mn5x2 |
Avg. Threshhold Voltage=0.765 |
Avg. Sigma=0.011 |
|---|
| Mn15x2 |
Avg. Threshhold Voltage=0.748 |
Avg. Sigma=0.010 |
|---|
| Mn10x3 |
Avg. Threshhold Voltage=0.745 |
Avg. Sigma=0.009 |
|---|
| Mn5x3 |
Avg. Threshhold Voltage=0.755 |
Avg. Sigma=0.012 |
|---|
| Mn15x3 |
Avg. Threshhold Voltage=0.740 |
Avg. Sigma=0.010 |
|---|
| Mn5x5 |
Avg. Threshhold Voltage=0.750 |
Avg. Sigma=0.010 |
|---|
| Mn10x5 |
Avg. Threshhold Voltage=0.739 |
Avg. Sigma=0.008 |
|---|
| Mn15x5 |
Avg. Threshhold Voltage=0.735 |
Avg. Sigma=0.008 |
|---|