Voltage for cmos58_Mp5x5 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.922125
2
-0.870715
4
-0.954046
6
-0.905916
7
-1.06303
8
-0.864872
9
-0.883498