Voltage for cmos58_Mp5x2 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.910675
2
-0.874485
4
-0.951492
6
-0.903595
7
-0.927145
8
-0.85834
9
-0.872401