Voltage for cmos58_Mp5x1.1 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.830949
2
-0.80657
4
-0.884091
6
-0.819785
7
-0.847693
8
-0.78915
9
-0.801658