Voltage for cmos58_Mp5x1.0 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.796943
2
-0.787861
4
-0.859771
6
-0.787786
7
-0.824249
8
-0.771084
9
-0.78152