Voltage for cmos58_Mp5x0.8 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.654234
2
-0.653402
4
-0.635829
6
-0.602028
7
-0.643571
8
-0.609261
9
-0.62168