Voltage for cmos58_Mp15x1.1 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.845191
2
-0.816236
4
-0.890239
6
-0.849496
7
-0.859893
8
-0.814436
9
-0.819159