Voltage for cmos58_Mp15x1.0 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.827506
2
-0.801226
4
-0.873863
6
-0.824579
7
-0.843097
8
-0.796936
9
-0.802887