Voltage for cmos58_Mp10x3 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.903313
2
-0.858574
4
-0.937226
6
-0.896047
7
-0.911386
8
-0.862184
9
-0.87298