Voltage for cmos58_Mp10x1.2 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.857454
2
-0.825436
4
-0.899711
6
-0.855401
7
-0.871349
8
-0.821352
9
-0.825542