Voltage for cmos58_Mp10x1.0 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.823973
2
-0.794124
4
-0.87104
6
-0.82426
7
-0.836117
8
-0.789304
9
-0.796644