Voltage for cmos58_Mp10x0.9 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.773306
2
-0.759845
4
-0.82663
6
-0.778972
7
-0.784995
8
-0.750255
9
-0.758382