Voltage for cmos58_Mp10x0.8 PVT
WAFER NUMBER
THRESHHOLD VOLTAGE
10
-0.680345
2
-0.673316
4
-0.739885
6
-0.672952
7
-0.678724
8
-0.671304
9
-0.68386