Step 53.
Via etch
|
Step |
Process |
Date |
Operator |
|
53.1 |
Etch rate ~2700A/min Etch time: 250sec (~20 sec over etch included) Check R on manual probe: 0.1-1Ohm -> down on M1. |
03/29/05 |
Horvath |