Step 48.
Metal 1 etch
|
Step |
Process |
Date |
Operator |
|
48.1 |
Standard recipe. Etch time: 1 min 25 sec + 50% OE. Check R with manual probe on field ox. area on each wafer to ensure Al is gone.
|
11/30/04 |
Horvath |