Crestec Dose Calculations

Dose resolution is 0.001 μs
Pixel Size 10.000 nm
Est. Beam Diameter -- nm

Calculate For:

Standard Formula: Dwell Time = (FieldSize/Dots)² * Sensitivity / Current